Customization: | Available |
---|---|
Application: | Industrial, Electronics |
Type: | Silicone |
Still deciding? Get samples of US$ 10/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Properties
|
Test Standard
|
BEGR 295
|
|
Appearance
|
/
|
White, translucent
|
|
Penetration
|
GB-T 269-1991
|
310 1/mm
|
|
Bleed, 30hours/200°C
|
HG/T 2502-1993
|
0.05 % Max
|
|
Evaporation, 30 hours/ 200°C
|
GB/T 2793-1995
|
1.15 % Max
|
|
Service temperature range
|
GB/T 2793-1995
|
-55 to +200 ºC
|
|
Relative density at 25°C
|
GBT 15223-1994
|
1.0 g/cm3
|
|
Dielectric strength, 1.27mm gap
|
GBT 1695-2005
|
18 kV/mm
|
|
Permittivity at 100Hz
|
GBT 1693-2007
|
2.90
|
|
Dissipation factor at 1000kHz
|
GB/T 5654-2007
|
<0.002
|
|
Dissipation factor at 100Hz
|
GB/T 5654-2007
|
0.002
|
|
Volume resistivity at 23°C
|
GBT 1692-2008
|
0.2 x 1015
|
|
Arc resistance
|
GB/T 1411-2002
|
120 seconds
|